TECHNOLOGIES
Investigation of extruded polyethylene blend films tensile creep elongation with different open holes configurations
Machines. Technologies. Materials., Vol. 19 (2025), Issue 1, pg(s) 30-32
In this article,tensile creep elongation of PE plastic films with two configurations of open holes stressed at the incremental temperatures of 23,30,37,43,51,58 degrees and a constant dead weight of 50 kg will be analyzed. The aim of the article is to analyze influence of the two configurations of open holes on the relative elongation. The test was conducted with the same blend, under the same test conditions. The test was conducted entirely according to the conditions established in the ASTM D6992 standard.