Keyword: pitting corrosion

  • THE RESISTANCE OF AISI 316Ti STEEL TO PITTING IN 1 M CHLORIDE ACIDIC SOLUTION IN THE ABSENCE AND PRESENCE OF INORGANIC INHIBITOR

    • Zatkalíková V.
    • Markovičová L.
    • Omasta M.
    • Oravcová M.
    Machines. Technologies. Materials., Vol. 10 (2016), Issue 1, pg(s) 36-38
    • Abstract
    • View Article
    •  Article PDF

    AISI 316Ti stainless steel is prone to local corrosion in aggressive chloride environments. Its resistance to pitting in the absence and presence of molybdate inhibitor was tested by two independent tests with different mechanisms of corrosion process: by exposure (24 hours immersion test) and electrochemically (potentiodynamic polarisation test). Both tests were carried out in 1 M chloride acidic solution without inhibitor and with two different amounts of added inhibitor (concentration ratio inhibitive/aggressive anions was 1:10 and 1:20 respectively), at room temperature. Results of immersion tests were evaluated on the bases of corrosion rates calculated from corrosion losses during immersion and by morphology of pitting. Results of potentiodynamic polarisation tests were evaluated by pitting potentials.

  • THE EFFECT OF FLUORIDE ON CORROSION BEHAVIOUR OF AUSTENITIC STAINLESS STEEL

    • Zatkalíková V.
    • Markovičová L.
    • Oravcová M.
    Materials Science. Non-Equilibrium Phase Transformations., Vol. 2 (2016), Issue 4, pg(s) 56-58
    • Abstract
    • View Article
    •  Article PDF

    Austenitic stainless steels are widely used for various industrial, construction and biomedical application because of their high resistance to uniform corrosion and suitable mechanical properties. However, they are prone to local corrosion in aggressive halides environments. In contrast of corrosion resistance research in chloride containing environments, there have been few investigations into the effect of fluorides on passivity breakdown and pitting corrosion of stainless steels. This article focuses on the effect of fluoride added to chloride solution on corrosion resistance of AISI 316L stainless steel. Evaluation is based on results of exposition immersion tests performed in 0.9 % NaCl, 0.9 % NaCl + 0.05 % NaF and 0.9 % NaCl + 0. 5 % NaF solutions (42 days) and on results of cyclic potentiodynamic polarization tests performed in the same solutions.

Congresses and conferences

  • International Scientific Conference
    "ARTIFICIAL INTELLIGENCE"
    07.03-10.10.2026 - Borovets, Bulgaria
  • IX International Scientific Conference
    "High Technologies. Business. Society"
    09.-12.03.2026 - Borovets, Bulgaria
  • XXIII International Congress
    "Machinеs. Technolоgies. Materials."
    Winter session
    11.-14.03.2026 - Borovets, Bulgaria
  • XXXI International Scientific Technical Conference
    "Foundry"
    22.-24.04.2026 - Pleven, Bulgaria
  • XXXIV International Scientific Conference
    "trans&MOTAUTO"
    22.-25.06.2026 - Varna, Bulgaria
  • XII International Scientific Congress
    "Innovations"
    22.-25.06.2026 - Varna, Bulgaria
  • XI International Scientific Conference
    "Industry 4.0"
    Summer session
    24.-27.06.2026 - Varna, Bulgaria
  • XV International Scientific Congress
    "Agricultural Machinery"
    24.-27.06.2026 - Varna, Bulgaria
  • XIV International Scientific Conference
    "Engineering. Technologies. Education. Safety"
    31.08-03.09.2026 - Varna, Bulgaria
  • X International Scientific Conference
    "Materials Science. Non-Equilibrium Phase Transformations"
    31.08-03.09.2026 - Varna, Bulgaria
  • XXIII International Congress
    "Machines. Technologies. Materials"
    Summer session
    02.-05.09.2026 - Varna, Bulgaria
  • X International Scientific Conference
    "POWER TRANSMISSIONS"
    02.-05.09.2026 - Varna, Bulgaria
  • XIX International Conference for Young Researchers
    "Technical Sciences. Industrial Management"
    11.-14.09.2026 - Varna, Bulgaria
  • XI International Scientific Conference
    "Conserving Soils and Water"
    07.-10.12.2026 - Borovets, Bulgaria
  • X International Scientific Conference on Security
    "Confsec"
    07.-10.12.2026 - Borovets, Bulgaria
  • XI International Scientific Conference
    "Industry 4.0"
    Winter session
    09.-12.12.2026 - Borovets, Bulgaria
  • V International Scientific Conference
    "Mathematical Modeling"
    09.-12.12.2026 - Borovets, Bulgaria

Powered by Tefterche.org

Scientific Technical Union of Mechanical Engineering "Industry-4.0"

108, Rakovski Str., 1000 Sofia, Bulgaria
tel. (+359 2) 987 72 90, tel./fax (+359 2) 986 22 40,
office@stumejournals.com