• MATERIALS

    The influence of aging parameters on thermal, mechanical and structural properties of the EN AW-6060 aluminum alloy

    Machines. Technologies. Materials., Vol. 18 (2024), Issue 1, pg(s) 29-32

    This paper investigates the influence of aging parameters (temperature and time) on thermal, mechanical and structural properties of the EN AW-6060 aluminum alloy. Thermal diffusivity and hardness were measured after applied heat treatments followed by investigation on scanning electron and transmission electron microscopes. Heat treatments included: solutionizing at 550°C for 1 hour followed by quenching in ice water; after quenching samples were aged at two separate temperatures of 180°C and 200°C for 1-8 hours. The results show that hardness gradually increases with aging time achieving peak value of 95 HV10 after aging at 180°C for 5 hours. Thermal
    diffusivity also increases with both aging time and temperature achieving peak values after aging at 200°C for 4 hours. SEM/EDS analysis show the existence of finely distributed precipitates containing Mg, Si and Fe. TEM investigation confirms the existence of rod-shaped precipitates several nanometers in length.

  • MATERIALS

    Investigation on durability testing of polyethylene (PE) geocells

    Machines. Technologies. Materials., Vol. 17 (2023), Issue 8, pg(s) 334-336

    In this article, the residual strength of PE geocells after accelerated aging is experimentally investigated. The characteristic is of key importance for the application of geocells, as it is related to their service life.The durability test is defined as essential in the applications standards of the product-EN 13 255:2016,EN 13 251:2016.

  • Impostation of an experimental design for studying the optimization of artificial aging process for the aluminium alloys

    Materials Science. Non-Equilibrium Phase Transformations., Vol. 7 (2021), Issue 3, pg(s) 85-88

    New area industry of Albania, in recent years, factories with closed cycle of production and processing of aluminium alloys are being targeted. In Albania about 25,000 tons of aluminum alloys per year are produced and there is a tendency to increase this production. This reality has encouraged us to undertake a number of studies with the primary objective for optimizing the parameters of the basic process of this industry. In this article we focus on the process of artificially aging aluminum alloys. From early and newer studies [2], the importance and delicacy of temperature-time parameters in the evolution of microstructure and in the mechanical properties of the final product are recognized and underlined. We have impost an experimental planning based on the Response Surface Method by choosing Central Composite Design to optimize the temperature and time parameters for the artificial aging with the object ive of maximizing the process indicator – mechanical properties, hardness in our case. The plan includes 13 tests with 5 replicas in the center of the experiment, built with the help of Design-Expert DX7 and DX13 software. The focus of our attention was the assesment of the design, analysis of residuals and diagnostic diagrams and forms of presentation of results: mathematical model, 3D response surface, isocontours and effects of interaction between factors. In the future works we will present the experimental results of the optimization of the artificial aging process for different aluminium alloys produced in Albania.

  • MATERIALS

    Formation of ZrB2-AlN powder mixture by self-propagating high-temperature synthesis

    Machines. Technologies. Materials., Vol. 13 (2019), Issue 9, pg(s) 414-416

    Formation of ZrB2-AlN mixed powder by self-propagating high-temperature synthesis (SHS) was investigated. Powders of Zr, B, BN and Al (purity >99 %) was used as the starting materials. Two initial mixtures were prepared and mixed at specific ratios. The first mixture was made of Zr and B, which were weighed at stoichiometric amounts to form ZrB2. The second mixture contained Zr, BN and Al; amounts of which were calculated so as to form ZrB2 and AlN.
    The starting powders were mixed in a mortar and pestle, and then the reactant mixture was slightly pressed in a steel die. The SHS reactions were conducted in high purity argon atmosphere, in an SHS chamber. The reactant pellet was ignited from one end with a tungsten wire. The reaction products were examined with scanning electron microscopy and they were subjected to X-ray diffraction analyses.
    It was found that when the reactants contained 40 % mixture-1 and 60 % mixture-2, according to the XRD results of the products, the peaks related to ZrB2 were dominant. The product contained some AlN and ZrN. When the amount of mixture-2 was increased to 90 %, the amounts of AlN and ZrN both were observed to increase. When Al amount in mixture-2 was increased by 30 % and mixture-2 was added as 90% into mixture-1, amount of AlN in the reaction products increased and amount of ZrN decreased. According to SEM examinations, ZrB2 particles were seen to be mixed with AlN particles in the reaction products. Size of ZrB2 particles were about 1 micron and AlN particles were larger.

  • MATERIALS

    Effect of aging on Zamak 3

    Machines. Technologies. Materials., Vol. 13 (2019), Issue 8, pg(s) 367-369

    Zamak 3 is a zinc-aluminum alloy with a composition of 3.7-4.3 %Al, <0.05 % Cu, 0.02-0.06 % Mg, rest is Zn. It is well suited for pressure die casting and it results in sufficient mechanical properties and a good surface finish. Zamak 3 is utilized in applications automotive industry, household appliances, in structural applications of buildings, etc. It was reported in literatüre that the mechanical properties of the zamak alloys deteriorate in time at room temperature. In the present study, this effect was investigated by artificial aging of zamak 3 alloy.
    Zamak 3 samples were produced by cutting and melting of Zamak 3 ingots at 500 oC, and casting into steel molds. Aging experiments were conducted by keeping the Zamak 3 samples in a muffle furnace for 24 h at temperatures of 85 oC, 105 oC and 130 oC. Optical and scanning electron microscopy was employed for investigating the microstructure of the samples. Hardness values of the samples were measured by a Brinell hardness tester. A universal testing machine was used for conduction three point bending tests of the samples. It was found that both hardness and bending strength of Zamak 3 alloy decreased with increasing aging temperature. Hardness and strength values of Zamak 3 were 89 HB10 and 490MPa, respectively. After aging at 130 oC hardness and strength values were found to fall to 75 Brinell 10 and 415 MPa, respectively.