MATERIALS

The Influence of Heat Treatment on Mechanical and Corrosion Properties of High- Chromium White Cast Irons Modified by Titanium and Boron

  • 1 University of Montenegro, Faculty of Metallurgy and Technology
  • 2 University of Belgrade, Faculty of Technology and Metallurgy

Abstract

The effect of individual additions of Ti and B into high chromium white cast irons (HCWCIs) on the structure, corrosion and selected mechanical properties was investigated. Two different heat treatments were applied, high-temperature treatment at 960 oC/1h, and subcritical treatment at 550 oC/4 h. The microstructure was investigated by OM and SEM; compositions of matrix and carbides were analyzed by EDS. Mechanical behavior of HCWCIs was analyzed by measuring hardness, toughness, abrasive/wear resistance and resistance to repeated impacts. Corrosion behavior was evaluated electrochemically, by linear and Tafel polarization methods in 0,1M NaCl solution. The properties of the modified HCWCIs were compared with the properties of the base unmodified HCWCI alloy (ASTM A532-IIE).

Keywords

References

  1. Kaya, S., et. all, Influences of Cr on the microstructural, wear and mechanical performance of high-chromium white cast iron grinding balls, Journal of Materials and Manufacturing Vol. 1 No. 1 (1:23-30), DOI:10.5281/zenodo.7107351 (2022)
  2. R.J. Chung, et al, Effects of titanium addition on microstructure and wear resistance of hypereutectic high chromium cast iron Fe–25wt.%Cr–4wt.%C, Elsevier, Wear 267 (2009) 356-361, DOI: 10.1016/j.wear.2008.12.061 (2009)
  3. High Alloy White Irons, Total Materia, ref.13 December 20, 2002
  4. Delijić K., Filipović M., The Effect of Vanadium, Niobium and Boron on Microstructure, Mechanical and Corrosion Properties of High-Chromium White Cast Irons, International Journal for Science, Technics and Innovations for the Industry, Issue 8/2022 pp. 286-289, ISSN 1314-507x (2022)
  5. Jain, A.-S., et all, Refinement of primary carbides in hypereutectic high-chromium cast irons: a review, Journal of Materials Science 56(2), 999-1038, (2021)
  6. Zhang, M.X., Kelly, P.M., & Gates, J.D., The effect of heat treatment on the toughness hardness and microstructure of low carbon white cast irons, J. Mater. Sci., 36, 3865–3875. (2001)
  7. Powell G.L.F., & Bee, J.V., Secondary carbide precipitation in an 18 wt% Cr–1 wt% Mo white iron, J. Mater. Sci., 31, 707– 711. (1996)
  8. Zhu, C., et all, Effect of boron addition on the microstructure and wear resistance of laser beam directed energy deposited high chromium white irons, Wear Volumes 546-547 1 June 2024, 205320, https://doi.org/10.1016/j.wear.2024.205320 (2024)
  9. Kaleicheva J., et all, Effect of boron on the wear behavior of high chromium white cast irons, Proc. of the 14th International Scientific and Practical Conference. Volume 3, 119-123 Print ISSN 1691-5402 Online ISSN 2256-070X https://doi.org/10.17770/etr2023vol3.7294 (2023)
  10. Naiheng M.A., Qichang R., Qingde Z. Corrosion-abrasion wear resistance of 28%Cr white cast iron containing boron Wear, 132 (1989), pp. 347-359, 10.1016/0043-1648(89)90083-5
  11. Z. Liu, Y. Li, X. Chen, K. Hu Microstructure and mechanical properties of high boron white cast iron Mater. Sci. Eng., A, 486, pp. 112-116, 10.1016/j.msea.2007.10.017 (2008)
  12. Y. Peng, H. Jin, J. Liu, G. Li Effect of boron on the microstructure and mechanical properties of carbidic austempered ductile iron Mater. Sci. Eng., A, 529, pp. 321-325, 10.1016/j.msea.2011.09.034 (2011)
  13. J. Hufenbach, K. et. all. The effect of boron on microstructure and mechanical properties of high-strength cast FeCrVC Mater. Sci. Eng., A, 586, pp. 267-275, 10.1016/j.msea.2013.07.085 (2013)
  14. M. Çöl, F.G. Koç, H. Öktem, D. Kır The role of boron content in high alloy white cast iron (Ni-Hard 4) on microstructure, mechanical properties and wear resistance Wear, 348–349, pp. 158-165, 10.1016/j.wear.2015.12.007 (2016)
  15. H. Lu, T. Li, J. Cui, Q. Li, D.Y. Li Improvement in erosion-corrosion resistance of high-chromium cast irons by trace boron Wear, 376–377, pp. 578-586, (2017)10.1016/j.wear.2017.02.014
  16. Chengbo Zhu et all, Effect of Ti and TiC additions on the microstructure and wear resistance of high chromium white irons produced by laser directed energy deposition, Wear Volumes 510–511, 15 December 2022, 204519, https://doi.org/10.1016/j.wear.2022.204519 (2022)

Article full text

Download PDF