• Photoluminescence properties of Sm3+-doped ZrO2–TiO2–Al2O3 coatings

    pg(s) 123-126

    The emission spectrum of the ZrO2–TiO2–Al2O3–Sm2O3 coating was recorded at different excitation wavelengths. Under UV excitation (λₑₓ = 354 nm), broad band with a maximum around 420–440 nm was observed and can be associated with oxygen vacancies in ZrO2 together with Ti³⁺ centers. Weakly intense and narrower emission bands at 600 nm and 647 nm are assigned to the 5G5/2  7H7/2 and 5G5/2  7H9/2 transitions of Sm3+ ions. Under excitation with 404 nm the emission is dominated by defect levels in the oxide coating. The values of the chromaticity coordinates of the coating excited under 354 nm correspond to the pale pink color of emission (0.252, 0.272) and under 404 nm has orange color of emission (0.353, 0.370).

  • Effect of non-metallic inclusions on the grain structure of low-carbon steels under severe plastic deformation

    pg(s) 77-80

    The features of localization of severe plastic deformation in a steel matrix near non-metallic inclusions are studied. In the steel matrix, near inclusions and at the inclusion-matrix interphase boundaries, the nature of the stressed and deformed states changes, the strain increment is determined by the rotation angle of the inclusion during its movement in the plastic region. Processes of local structural transformations near non-metallic inclusions in steels exposing to intensive plastic deformation were investigated. The influence of non-metallic inclusions on the local refinement of the steel microstructure is an important effect during severe plastic deformation, which makes it possible to obtain additional nanostructural strengthening near the inclusions during the general refinement of grains to a submicrocrystalline state. It was shown the influence of non-metallic inclusions on mechanical properties of these steels.

  • Comparative Analysis of Natural Ruby and Synthetic Corundum Ceramics by UV–Vis and Raman Spectroscopy

    pg(s) 73-76

    This study presents a comparative spectroscopic investigation of natural Cr³⁺-bearing ruby and multiphase Al₂O₃-based ceramics derived from industrial waste. The natural corundum shows characteristic Cr³⁺ crystal-field absorption bands at ~405 and ~550 nm and sharp R-line emission near 693 nm, confirming a structurally ordered α-Al₂O₃ lattice. In contrast, the waste-derived ceramics exhibit charge-transfer-dominated absorption associated mainly with V⁵⁺ and Fe³⁺ under oxidizing firing conditions. Strong UV absorption (220–300 nm) and the absence of vanadium crystal-field transitions indicate predominant V⁵⁺ stabilization, consistent with chemical and phase analysis. The ceramics display high lightness (L* ≈ 93) and a yellow hue (b* = 10–23) governed by ligand-to-metal charge-transfer processes. The results demonstrate the effectiveness of combined UV–Vis and Raman spectroscopy for distinguishing crystal-field and charge-transfer mechanisms and for resolving dopant-related colour formation in alumina systems.

  • Development of an All-Optical Platform for Real-Time Monitoring of Hypoxia Dynamics

    pg(s) 69-72

    Oxygen levels in the cellular microenvironment, particularly under hypoxic conditions, play an active regulatory role in modulating cellular function, signaling pathways, and metabolic networks. A radically new concept for sensing the oxygen concentration at the extracellular liquid microenvironment was developed, based on nanoconfined upconversion optical sensors. The experimental achievements in developing technologically applicable strategies for minimally invasive monitoring of the oxygen concentration in cell microenvironment will be presented and discussed.

  • Fermented grape pomace ash – by-product of rakia (brandy) production

    pg(s) 38-44

    This study investigates the chemical, mineralogical, and functional characteristics of fermented grape pomace ash generated after brandy production and subsequent combustion. Semi-quantitative WDXRF analysis revealed a Ca–K–P-dominated composition with high alkalinity, significant phosphorus content, and notable copper concentration. The water-soluble fraction of the ash was determined to be 17.1 wt.%, indicating a moderate content of mobile inorganic salts that may influence leaching behaviour and environmental compatibility. XRD and vibrational spectroscopy confirmed the presence of lime, calcite, silicates, sulphates, and calcium phosphate phases, including hydroxyapatite, together with a significant amorphous fraction and residual carbon. UV–Vis analysis indicated partial reduction of copper species to metallic nanoparticles, suggesting heterogeneous redox conditions during thermal treatment. The combined composition confers potential functionality in soil amendment, mineral carbonation for CO₂ sequestration, and incorporation into cementitious or alkali-activated systems, although soluble salts and copper mobility represent critical constraints, requiring application-specific environmental and performance assessment.

  • Structure and properties of AlB12-Al detonation coatings on Steel 45

    pg(s) 34-37

    The work is dedicated to the study of the properties of detonation coatings AlB12-30 wt.% Al (AB70) applied to Steel 45 using the DNEPR-5M installation. The coatings have the following characteristics: thickness h ~ 170-200 μm, Hμ = 27-29 GPa, HV = 4.35 GPa. Changes in the tribological characteristics of the composite depending on the friction mode are analyzed. The AB70 coating is found to have stable tribological characteristics: f = 0.21-0.38, wear rate I = 3.3-8.6 μm/km. Samples with coatings exceed uncoated Steel 45 in wear resistance. Changes in the surface structure after friction depending on the sliding speed and load are shown. Two wear mechanisms – oxidative and adhesive-abrasive – are established. A conclusion was drawn regarding the possibility of using the AlB12-Al system to apply detonation coatings.

  • Observed Damage Patterns and Material Strength Deficiencies in URM Dwellings After the 2019 Albania Earthquake

    pg(s) 30-33

    This paper investigates the link between earthquake damage and material strength deficiencies in four unreinforced masonry (URM) dwellings in Kruja, Albania, which all reached Damage State 4 (DS-4) during the Mw 6.4 earthquake of 26 November 2019. Post-earthquake field inspections showed similar failure patterns in all buildings, including diagonal shear cracking, corner separation and local out-of-plane instability, pointing to limited shear capacity and weak masonry bonding.
    To clarify the causes of this behaviour, laboratory tests were carried out on brick units, mortar samples and masonry prisms taken from the damaged buildings. The test results indicate that both mortar and masonry compressive strengths are significantly lower than the values commonly assumed in Eurocode 6 for structural assessment. This strength deficit explains the brittle response and the rapid stiffness degradation observed during the earthquake.
    The combined use of field observations and laboratory data confirms the key role of construction quality in the seismic vulnerability of older URM dwellings and underlines the importance of material-based assessment approaches for similar residential buildings.

  • Influence of femtosecond laser processing parameters on the surface morphology of titanium alloy

    pg(s) 26-29

    Titanium alloys are essential in biomedicine due to their high specific strength and biocompatibility, with surface properties directly influencing the successful osseointegration of implants. In this study, surface texturing of an experimental titanium alloy was performed using an ultrafast femtosecond laser with varying pulse energies. Roughness and topography were analysed using optical profilometry and confocal laser scanning microscopy, while microhardness was measured by the Vickers method. The results show that a pulse energy of 2.1 µJ, with a wavelength of 1030 nm, pulse duration of 190 fs, and repetition rate of 1 MHz, constitutes the optimal laser process parameters for achieving the desired surface properties in engineering and biomedical applications.

  • Phenomena during liquid-phase assisted sintering in High-Entropy Ceramics with a Ni binder

    pg(s) 479-482

    This study investigates the mechanisms of liquid-phase assisted sintering in high-entropy ceramics (HECs) using a nickel binder. The research focuses on the densification process of (Ti, Zr, Hf, Nb, Ta)C-based cermets with 10 vol% Ni, and how pressure influence liquid-phase extraction. Results show that eutectic reactions between Ni and carbide phases was observed during liquid formation below 1400°C. Microstructural analysis reveals a nickel-rich matrix, solid solutions, and NbC-based carbide inclusions in the extracted drop. These findings provide insights into optimizing processing parameters for advanced HEC-based composites.

  • Optical and microstructural properties of hybrid sol–gel derived ZrO₂–Al₂O₃–Sm₂O₃ coatings on glass for photovoltaic applications

    pg(s) 476-479

    This work presents an overview of sol–gel-derived oxide materials and their relevance to optical, photonic and photovoltaic applications, followed by an experimental study of ZrO₂–Al₂O₃–Sm₂O₃ thin films deposited on glass substrates. Historical developments of the sol–gel process, beginning with early investigations on silica gels in the 19th century, are outlined together with advancements in optical glasses, anti-reflective coatings, and rare-earth-doped systems. Recent progress in functional materials—including boron-, tellurium- and rare-earth-containing glasses, luminescent oxide systems, and sol–gel-derived zirconia-based coatings—is discussed to highlight their structural, optical and radiation-shielding capabilities.
    In the present study, multilayer ZrO₂–Al₂O₃–Sm₂O₃ coatings were prepared via the sol–gel method combined with dip-coating, and subsequently thermally treated at 420 °C. Optical characterization (UV–VIS–NIR) revealed changes in transmittance and reflectance linked to film composition and thickness, while X-ray diffraction confirmed their predominantly amorphous structure at the applied heat-treatment temperature. SEM and EDS analyses provided insight into surface morphology and elemental distribution within the films. The results demonstrate that increasing Al₂O₃ content influences coating porosity and thickness, while Sm₂O₃ contributes luminescent functionality and potential reduction of optical reflection in key solar spectral regions. These findings indicate that ZrO₂–Al₂O₃–Sm₂O₃ thin films are promising candidates for protective and functional coatings in photovoltaic applications, where enhanced light harvesting and improved surface properties are essential.

  • Investigation of the corrosion resistance of composite ZrO2–Al2O3–Sm2O3 films obtained by sol-gel method on aluminum alloy A356

    pg(s) 449-451

    Corrosion remains a major limitation for the long-term use of aluminum alloys such as A356, particularly in chloride-rich environments. Although traditional chromate coatings provide effective protection, their toxicity necessitates environmentally friendly alternatives. In this study, a composite ZrO2–Al2O3–Sm2O3 coating was synthesized via a sol-gel method and deposited on A356 alloy using dip-coating. The precursor system was formulated from zirconyl chloride, samarium oxide, and aluminum oxide, stabilized with acetylacetone and acetic acid at pH 0.5 to ensure homogeneous film formation. The coated samples were thermally treated at 400 °C to obtain dense oxide layers. Corrosion resistance was assessed under neutral salt spray conditions (5% NaCl, 35 °C, 648 h) according to BDS EN ISO 9227:2023. Comparison between uncoated A356, binary Al–Zr (ADZ), and ternary Sm–Al–Zr (SADZ) coatings demonstrated a clear performance improvement with increasing film complexity. While ADZ coatings reduced surface damage relative to the bare alloy, the SADZ films exhibited the lowest amount of corrosion products, minimal surface darkening, and significantly reduced pitting. The enhanced performance is attributed to the synergistic effect of the three oxides: ZrO₂ provides chemical stability, Al2O3 increases layer density, and Sm₂O₃ contributes active corrosion inhibition.
    Overall, the ZrO2–Al2O3–Sm2O3 composite film offers a promising non-chromate protective system for improving the long-term corrosion resistance of A356 aluminum alloy.

  • Multicore Iron Oxide Nanoflowers as Smart Functional Materials for Catalytic Technologies

    pg(s) 448-448

    Multicore iron oxide nanostructures (“nanoflowers”) have emerged as a unique class of functional materials whose properties cannot be explained by simple extrapolation from single-core nanoparticles. Their hierarchical architecture, consisting of primary crystallites coupled into coherent multicore assemblies (Fig. 1a), enables the engineering of magnetic, structural and surface phenomena often unachievable in single-core nanoparticles. In the context of Industry 4.0, where advanced materials must integrate high performance, configurability, multifunctionality, and compatibility with digital platforms, such nanostructures offer significant potential for catalytic and environmental applications.
    In a series of recent and ongoing studies, we have systematically investigated how material composition, defect structure, surface chemistry, synthesis conditions, and multicore organization govern the functional properties of iron oxide nanoflowers. By integrating structural analysis (XRD), electron microscopy (TEM), XPS spectroscopy, magnetic characterization (SQUID), and calorimetric measurements under AC magnetic fields, we have established a unified framework for the design and optimization of these materials. A particular focus of our research is the surface chemistry and ability of these nanostructures to generate heat under AC magnetic fields (magnetic hyperthermia).
    The successful design of materials with well-defined surface redox pairs and high hyperthermic efficiency enables their use as heterogeneous catalysts for the degradation of emerging organic pollutants.
    Our previously published work on Gd3+-doped γ-Fe2O3 nanoflowers demonstrated that even very low doping levels (≤1.7 mol%) induce pronounced surface and bulk modifications while preserving the maghemite phase and multicore morphology [1]. Gd3+ incorporation generates redox-active surface defects, increases the Fe2+ fraction, promotes oxygen-vacancy formation, enhances magnetic anisotropy, and strongly influences magnetic hyperthermia efficiency [1]. These results demonstrate that controlled defect engineering within multicore architectures enables tuning of magnetic heating and surface ionic composition, which is essential for achieving multifunctional performance. Complementary work on Zn/Mn-modified γ-Fe2O3 nanoflowers has shown that heterovalent substitution leads to vacancies at octahedral sites within the spinel lattice, resulting in pronounced local structural distortions [2]. These defect-rich multicore nanostructures exhibit exceptional magnetic heating performance, with SAR values reaching 369 W/g and ILP values up to 5.77 nH·m2/kg [2].
    Our ongoing work on optimizing polyol synthesis parameters shows that the reaction duration strongly influences crystallization behavior, particle aggregation, and the resulting hyperthermic performance of iron oxides. Nanoflowers synthesized at the optimal reaction time (4 h) exhibit high crystallinity, the smallest core sizes, the lowest coercivity, and the highest SLP/ILP values (Fig. 1b,c), confirming that process engineering plays a critical role in controlling functional properties. The surface and thermal characteristics of multicore iron oxide nanostructures are particularly important for their implementation in catalytic and environmental technologies. In our ongoing studies, we employ oxone (peroxymonosulfate) as a precursor of sulfate radicals, while the high heating efficiency of the nanoflower structures under
    AC magnetic fields enables rapid and selective oxone activation. This synergistic effect, combining enhanced surface redox activity with localized heating under the AC field, is expected to significantly accelerate the degradation of the model pollutant Reactive Black 5.